Ceramic (Chrome Oxide) Spray Coating

- Electrical Resistivity - Provides longer life span - High Hardness - High Durability - Anti-Galling - Dense and pore free

Flywheel (Dia.1.6m x Height 320mm) - Thermal spray repair worn out bearing seat Dia.320mm

Thermal spray repair worn out bearing seat Dia.320mm